Silvertone 1831 Restoration - Hagstar Studios
Here's the chassis after cleaning and degreasing with Lectra-Motive spray including wire brushing/Scotchbriting, and treatment with Permatex Rust Treatment at the back edge. The masking takes a few hours. Factory treatment was copper plating with silver paint. Rustoleum Stainless Steel like I used on the Grunow 1291 is again a good match for this.

Here's the chassis after cleaning and degreasing with Lectra-Motive spray including wire brushing/Scotchbriting, and treatment with Permatex Rust Treatment at the back edge. The masking takes a few hours. Factory treatment was copper plating with silver paint. Rustoleum Stainless Steel like I used on the Grunow 1291 is again a good match for this.